Liseo 01-30-2021 08:56 AM

Derimming die steel
 
Hi

I'm making some 224 bullets out of 22 lr cases.
But the derimming die insert is short-lived, has a lot of wear.
I'm thinking of making one, but I don't know which steel is more suitable, because I made a unit with silver steel(52100) and the useful life was short, because it had quick wear, even after doing the temper.

could someone give a tip?

Thanks

Hog Patrol 01-30-2021 12:38 PM

Do you have or have access to a heat treating oven/furnace? If so, A2 or O2.

gunhaus 02-11-2021 11:02 AM

I have made these for a number of years with 0-1 or O-6 both give great life. Also, pre-cleaning spent cases with on of the SS pin systems can dramatically increase life as the cases get VERY clean with this process. This with the sufficient and even distribution of a good swage lube will really increase the life of the dies.

TinMan 02-11-2021 01:46 PM

As I recall, AISI 52100 is a bearing steel.